Veneers from high quality logs are mechanically dried and they undergo stress relieving process, which are assembled in such a way to form a balanced construction. High quality fortified synthetic resins are used for gluing the veneers. Glue line is poisoned by special formulations of
chemicals to make Woodlyte Plywood safe against borers. It is hot pressed under proper temperature and more than 16 Kg/cm2 specific pressure. Conditioning is done after pressing, followed by preservative treatment.
Applications:
Partition and paneling, ceilings in public rooms and corridors, floor underlayment, computer rooms, furniture, bus bodies, railway coaches, milk booths, sign boards, insert in panel doors, storage racks.
Technical Specifications:
Title | Required Value | Observed Value |
Moisture Contents | 5%-15% | As per ISI Req. |
Dimension | Length +5mm, Width+2mm Thickness2-8mm + 5%, <6mm + 10% | With Limit |
Sp. Gravity | As per ISI Req. | |
Resistance to Water(3 cycles of 8 hr boiling & 16 HR. Drying at 65oC) -Adhesion to plies | Min. Pass Standerd | Excellent |
Resistance to Micro-organism -Adhesion to plies | Min. Pass Standard | Excellent |
Static Bending Test a) Modulus of Elasticity along the grain Avg. accross the grain Avg. b) Modulus of Rupture along the grain Avg. across the grain Avg. | Min. 5000 N/sq.mm Min. 2500 N/sq.mm Min. 40 N/sq.mm Min. 20 N/sq.mm | As per ISI Req. As per ISI Req. As per ISI Req. As per ISI Req. |